Sodium Nickel Iron Manganese Oxide Cathode Sheet (NT0103) Single-sided, 5 pieces/pack
Sodium Nickel Iron Manganese Oxide Cathode Sheet (NT0103) Single-sided, 5 pieces/pack
Sodium Nickel Iron Manganese Oxide Cathode Sheet (NT0103) Single-sided, 5 pieces/pack

CNB-2-CS20

Sodium Nickel Iron Manganese Oxide Cathode Sheet (NT0103) Single-sided, 5 pieces/pack

Regular price $143.00
/
Size

Product Name & Description

Sodium Nickel Iron Manganese Oxide Cathode Sheet (NT0103) is based on Aluminum foil coated by Sodium Nickel Iron Manganese Oxide (NT0103) on a single side and can be used as the cathode of sodium ion battery.

Initial Charge and Discharge Test Conditions:

  • Temperature: 25°C
  • Charge: First, charge at a constant current of 0.1C to 4.0V, then charge at a constant voltage until the current drops below 0.02C.
  • Discharge: Discharge at a constant current of 0.1C to 2.0V.

Rate Performance Test Conditions:

  • Temperature: 25°C

  • Charge: First, charge at a constant current of 0.5C to 4.0V, then charge at a constant voltage until the current drops below 0.02C.
  • Discharge: Discharge at constant current rates of 0.1C, 0.2C, 0.5C, 1C, 2C, and 3C to 2.0V.

Cycle Test Conditions:

  • Temperature: 25°C
  • Charge: First, charge at a constant current of 0.5C to 4.0V, then charge at a constant voltage until the current drops below 0.02C.
  • Discharge: Discharge at a constant current of 1C to 2.0V.

The electrolyte used for the performance data is: sodium electrolyte MA-EN-EL-0P0616 1.0M NaClO4 in EC: DEC=1:1 Vol% with 5.0% FEC

Specification

Material

Sodium Nickel Iron Manganese Oxide

Sheet Size (cm)

10*10

Current Collector Thickness (μm)

12

Current Collector Areal Density (mg/cm2)

3.30

Coating Areal Density (mg/cm2)

8.0

Active Material Specific Capacity (mAh:g)

120mAh/g

Active Material Ratio (%)

94.0

Recommended Compaction Density (g/cc)

2.0~2.5

Test Conditions 
(Room Temperature 25 ℃)

0.1/0.1C, 2.0-4.0V

Shelf Life

1/2 year (vacuum sealed storage),
use within 1 month after opening

Instructions For Use

1. The electrode calendering, needs to be calendered according to the recommended compaction density.
2. The surface density needs to be determined based on the actual weighing results.
3. Before placing it in the glove box, the electrodes needs to be vacuum dried at 105 ℃ for 4 hours


Note: Since the electrodes are single-side-coated, calendering may cause curling issues. 

 

Download Material Safety Data Sheet:


Download Technical Data Sheet:

Why Choose Beyond Battery?

Packed with Care

Your selected purchases are inspected and packed with care and consideration, both for the receiver and the handler.

30-Days Satisfaction Promise.

We work tirelessly to improve our products and services. If you are not satisfied with our product, contact us within 30-days of your purchase and let us make it up to you!

A Global
Provider

Reach out to us from wherever you are.